Dow DOWLEX® IP-90 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Next Generation DOWLEX® IP-90 resin is a high flow improved processing high density polyethylene resin designed for ultra-thin wall injection molded containers and drink cups. This resin has been molded into containers exceeding flow length/container wall thickness ratios of 350, while demonstrating good impact and load properties. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.1(a) for food contact applications. The regulation should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact Resistance
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|