Dow HDPE 08454N High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: Dow PE
Material Notes: DOW HDPE 08454N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness, with good stiffness. This resin has good processability over a wide range of molding conditions. Typical applications are in structural foams, industrial containers, cases/crates etc. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. Data provided by Dow Chemical.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact Resistance
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|