Dow HDPE 30460M High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: Dow PE
Material Notes: DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent processability over a wide range of molding conditions. Typical applications are thin wall containers, overcaps, and general purpose applications. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. Data provided by Dow Chemical.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact Resistance
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|