Dow LDPE 4012 Low Density Polyethylene, Extrusion Coating Grade
Subcategory: Polyethylene; Thermoplastic; LDPE
Key Words: Dow PE
Material Notes: DOW Polyethylene 4012 extrusion coating resin is used for thin coatings in applications such as sugar pouches, ice cream bar covers, easy tear packages, and freezer papers. It is designed to be run at high speeds and low coating temperatures. It complies with U.S. FDA regulation 21 CFR 177.1520 c 2.1 for food contact applications. The regulation should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Vicat Softening Point
|
|
|
|
| Property Data |