Dow LDPE 722M Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LDPE
Key Words: Dow PE
Material Notes: DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include caps/closures. This resin has good processability over a wide range of molding conditions. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched, Low Temp (ISO)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|