Dow SARAN® 416 PVDC
Subcategory: PVDC; Thermoplastic
Key Words: Polyvinyl Dichloride
Material Notes: SARAN® 416 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, is designed for extrusion and coextrusion into barrier films used in both food and medical packaging applications. It is supplied as a white, partially formulated free flowing powder (particle size 195-300 microns). It offers excellent oxygen and moisture barrier and complies with requirements of FDA for use as a component of articles in contact with food. Data provided by Dow Chemical.
| Available Properties |
- Density
- Oxygen Transmission
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|