Dow SARAN® 510 PVDC
Subcategory: PVDC; Thermoplastic
Key Words: Polyvinyl Dichloride
Material Notes: SARAN® 510 resin is a copolymer of vinylidene chloride and vinyl chloride, supplied as a white free flowing powder (particle size 250 microns). It is a formulated polymer designed for extrusion into mono filaments used for weaving of fabrics and filter clothes. It offers chemical and abrasion resistance along with ignition resistance. Data provided by Dow Chemical.