Dow SARAN® 867 PVDC
Subcategory: PVDC; Thermoplastic
Key Words: Polyvinyl Dichloride
Material Notes: SARAN® 867 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for extrusion and coextrusion into barrier films used in flexible packaging applications for food. It is supplied as a white free flowing powder (particle size 210-290 microns). It offers good oxygen barrier, excellent moisture barrier, and complies with the requirements of FDA for use as a component of articles in contact with food. Data provided by Dow Chemical.
| Available Properties |
- Density
- Oxygen Transmission
|
|
|
|
| Property Data |