Dow SARAN® F-239 PVDC
Subcategory: PVDC; Thermoplastic
Key Words: Polyvinyl Dichloride
Material Notes: SARAN® barrier resin F-239 is used for coating cellophane and polyester film. It is applied from a tetrahydrofuran/toluene solvent system, and gives coatings with excellent adhesion and transparency. Data provided by Dow Chemical.
| Available Properties |
- Density
- Oxygen Transmission
|
|
|
|