Dow SARAN® MA 119 PVDC
Subcategory: PVDC; Thermoplastic
Key Words: Polyvinyl Dichloride
Material Notes: SARAN® MA 119 barrier polymer with a molecular weight of 90000, is a copolymer of vinylidene chloride and methyl acrylate, designed for multilayer barrier films used in flexible packaging. It is supplied as a white, unformulated, free flowing powder (particle size 245 microns). It offers excellent oxygen and water vapor barrier, high shrink and complies with the requirements of FDA for use as a component of articles in contact with food (21 CFR 177.1990). Data provided by Dow Chemical.
| Available Properties |
- Density
- Oxygen Transmission
|
|
|
|