Solutia VYDYNE® 24HNSP Nylon, Nucleated, Heat Stable
Subcategory: Nylon; Thermoplastic; Nylon 66
Key Words: Polyamide 66, Nylon 6/6, Nylon 6,6; PA66
Material Notes: Typical property data. VYDYNE is a registered trademark of Solutia Inc.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|