Styrofoam™ Polystyrene Rigid Foam Insulation
Subcategory: Polystyrene
Key Words: Compare to Expanded Polystyrene (EPS); Dow Chemical
Material Notes: The information below is typical of Styrofoam™ rigid polystyrene foam used for construction insulation - but many specific grades are available. This material is produced as sheets of closed-cell foam by a continuous extrusion process. Its properties will be different than expanded polystyrene beads because beads have voids between cell walls. Styrofoam is a trademark of Dow Chemical.
| Available Properties |
- Density
- Water Absorption
- Compressive Yield Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|