Dyneon™ 1700 Modified PTFE Powder
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Key Words: Polytetrafluoroethylene; Dyneon PTFE
Material Notes: Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generation PTFE, but with a significantly lower melt viscosity giving better particle fusion during sintering and smoother surfaces. Dyneon TFM 1700 PTFE is a non-free-flowing compression molding powder and base material for high-quality Dyneon TFM PTFE compounds.Data provided by Dyneon.
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|