Dyneon™ 1605 Modified PTFE Powder
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Key Words: Polytetrafluoroethylene; Dyneon PTFE
Material Notes: Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon.
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|