Dyneon™ 1645 PTFE Powder
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Key Words: Polytetrafluoroethylene; Dyneon PTFE
Material Notes: Type IV, gr. 2 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:- Inert to a wide range of aggressive chemical agents
- Ultra-low friction coefficient
- Continuous service temperature range from cryogenic -330°F to 500°F
- Extremely resistant to embrittlement, aging or weathering
PTFE has rapidly become the material choice where low friction, high durability, excellent thermal resistance and chemical inertness characteristics are required. Data provided by Dyneon.
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Electrical Resistivity
- Surface Resistance
- Dielectric Strength
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|