Dyneon™ TF 2071 PTFE Paste Extrusion Powder
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Key Words: Polytetrafluoroethylene; Dyneon PTFE
Material Notes: Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1600. Average particle size 500 µm. Used for tubing, wire/cable insulation, 'spaghetti tubing' production. Dyneon offers a family of PTFE fine powder paste extrusion resins. These products are well suited for a variety of applications, including tubing, hose, pipe liners, tapes, wire and cable, diaphragms and textile/fiber. Available grades are designed to balance process properties such as reduction ratio, and performance properties, such as tensile strength, shrinkage, flex life and permeations. Data provided by Dyneon.
| Available Properties |
- Density
- Apparent Bulk Density
- Tensile Strength, Ultimate
- Elongation at Break
- Electrical Resistivity
- Surface Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|