Dyneon™ CC698 PTFE, 20% Fiberglass/Carbon Filled
Subcategory: Fluoropolymer; Thermoplastic; PTFE; Polymer
Key Words: Polytetrafluoroethylene; Dyneon PTFE
Material Notes: Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Yield Strength
- Compressive Yield Strength
- Compressive Modulus
- Coefficient of Friction
- Coefficient of Friction, Static
- K (wear) Factor
- CTE, linear 20°C
|
|
|
|