Dyneon™ TF 4220 PTFE, 2% Cond. Pigm. Filled
Subcategory: Fluoropolymer; Thermoplastic; PTFE; Polymer
Key Words: Polytetrafluoroethylene; Dyneon PTFE
Material Notes: Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon.
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Electrical Resistivity
- Surface Resistance
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
|
|
|
|