Dyneon Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Key Words: Vinylidene Fluoride, PVF2; Hexafluoropropylene; fluoropolymer, carbon black
Material Notes: Data provided by the manufacturer, Dyneon LLC. Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosphonium Accelerator. Improved elongation retention after long-term heat aging. Improved acid and organic solvent resistance. Blends with incorporated cure grades. Used in Raw Gums.
| Available Properties |
- Density
- Oxygen Transmission
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Coefficient of Friction
- Compression Set, Elevated Temperature
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|