Dynasol Calprene® 248 Medium CIS Polybutadiene (38%)
Subcategory: Elastomer, TS; Thermoset
Material Notes: Calprene 248 is a medium CIS polybutadiene (38 %), polymerized in solution. This product has an excellent mixing and processing behavior. It is used as ingredient in tire compounds and in other applications where good performance at low temperatures, excellent abrasion resistance, low heat build-up and good dynamic fatigue resistance are needed. It is packed in bales wrapped in low melting point polyethylene film. Applications: - Tires
- Mechanical rubber goods
- Plastic modifications
- Blends with other polymers
Compound Test Recipe: ISO-2476 (A). IBR #7 Information provided by Dynasol.
| Available Properties |
- Mooney Viscosity
- Ash
- Collected Volatile Condensable Material
- Tensile Strength at Break
- 300% Modulus
- Gel Content
- Hunterlab Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|