Dynasol Calprene® 375 Solution Random SBR
Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset
Material Notes: Calprene 375 is a Butadiene/Styrene Copolymer, polymerized in solution. It has a random structure with a typical vinyl content of 30%, and is extended with 37.5 phr of naphthenic oil. C-375 is used as ingredient in compounds for battery cases, tires, cables, vulcanized shoe soles and industrial rubber goods. It can replace SBR 1707, 1708, 1778 types. The bales are wrapped in low melting point polyethylene film. Applications: - Tires
- Footwear
- Mechanical rubber goods
Compound Test Recipe: ISO-2322 (A) Information provided by Dynasol.
| Available Properties |
- Mooney Viscosity
- Ash
- Collected Volatile Condensable Material
- Tensile Strength at Break
- Elongation at Break
- 300% Modulus
- Hunterlab Color
- Oil
- Total Styrene (on polymer)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|