Dynasol Calprene® 1204B Solution Random SBR
Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset
Material Notes: Calprene 1204B is a 75/25 Butadiene/Styrene Copolymer, polymerized in solution. It has a random structure with a typical vinyl content of 30%. It is presented in bales wrapped in low melting point polyethylene film. Applications: - Tires
- Footwear
- Mechanical rubber goods
Compound Test Recipe: ISO-2322 (A) Information provided by Dynasol.
| Available Properties |
- Mooney Viscosity
- Ash
- Collected Volatile Condensable Material
- Tensile Strength at Break
- Elongation at Break
- 300% Modulus
- Hunterlab Color
- Total Styrene (on polymer)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|