Dynasol Solprene® 375 Solution Random SBR
Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset
Material Notes: Solprene 375 is a tin coupled, random styrene-butadiene copolymer with 24% styrene content. It is extended with naphtenic oil. S-375 is used as ingredient in compounds for battery cases, tires, cables, vulcanized shoe soles and industrial rubber goods. It can replace SBR 1778 types. The bales are wrapped in low melting point polyethylene film. Information provided by Dynasol.
| Available Properties |
- Density
- Mooney Viscosity
- Ash
- Collected Volatile Condensable Material
- Tensile Strength at Break
- Elongation at Break
- 300% Modulus
- Antioxidant Content
- Free Soap
- Naphtenic Oil
- Organic Acid
- Styrene Content
|
|
|
|