Dynasol Calprene® 487 Thermoplastic Rubber SBS Oil extended
Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic; Styrenic TPE
Material Notes: Calprene 487 is a 45/55 Butadiene/Styrene thermoplastic copolymer, polymerized in solution. It has a
radial structure and is extended with 40 phr of paraffinic oil.This product is presented in pellet form and has very adequate flow properties for compounding articles intended for injection. Applications: - Footwear
- Sportswear
- Mechanical rubber goods
Information provided by Dynasol
| Available Properties |
- Volatiles
- Melt Flow
- Ash
- Styrene Content
- Hardness, Shore A
- Abrasion
- Hunterlab color, max
- Insolubles in toluene, 325 mesh, % max
- Oil Content, %
|
|
|
|