Dynasol Calprene® 540 Thermoplastic Rubber SBS Dry
Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic; Styrenic TPE
Material Notes: Calprene 540 is a 60/40 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure. This product is presented in pellet form and has excellent optical properties, due to its clarity. It is stabilized with a non staining antioxidant system FDA approved for use in food contact applications and is essentially gel free with a very clear color. C-540 is used in adhesive formulation, in thermoplastic injected shoe sole formulations, and transparent compounds.Applications: - Footwear
- Adhesives
- Plastic modification
Information provided by Dynasol
| Available Properties |
- Volatiles
- Brookfield Viscosity
- Melt Index of Compound
- Ash
- Styrene Content
- Hardness, Shore A
- Abrasion
- Hunterlab color, max
- Insolubles in toluene, 325 mesh, % max
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|