Dynasol Solprene® 1322 Styrene-Butadiene Rubber SBR Diblock Copolymer

 

Subcategory: Polystyrene; Elastomer, TPE; Styrene-Butadiene; Styrenic TPE

Material Notes:
Solprene 1322 is a high molecular weight linear random -block styrene-butadiene copolymer having 30% of styrene content, 22% present as a polystyrene block. It has a non-staining antioxidant system, FDA approved for use in food contact applications. It is a high purity polymer, essentially gel free with a very clear color. Solprene 1322 is used as an elastomeric impact modifier for plastics, especially in high gloss HIPS and ABS by the “in situ” polymerization process. It is available in bales wrapped in rubber-modified polystyrene film soluble in styrene monomer.

Applications:

  • Plastic modification

Information provided by Dynasol

Available Properties
  • Specific Gravity
  • Volatiles
  • Viscosity Measure
  • Styrene Content
  • Color Alpha, max
  • Insolubles in toluene, 325 mesh, % max
  • Monsanto gel, grade max
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。