Dyneon™ Fluorothermoplastics FEP 6307 R2R Fluorinated Ethylene Propylene
Subcategory: Fluoropolymer; Thermoplastic; FEP
Material Notes: Dyneon FEP 6307 R2R is a special version of Dyneon FEP 6307 wire jacketing grade FEP with an added nucleating agent for improved foaming in gas injection extrusion processes. As the gas expands and begins to form voids, the added nucleating agent in Dyneon FEP 6307 R2R acts as a site for void formation. Dyneon FEP 6307 R2R is listed by Underwriters Laboratories as a Plenum Cable Component. It is ideal for gas injection extrusion of foamed FEP coaxial cable core.Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Melt Index of Compound
- Dielectric Constant
- Dissipation Factor
- Melting Point
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|