Dyneon™ Fluorothermoplastics FEP 6322 Fluorinated Ethylene Propylene
Subcategory: Fluoropolymer; Thermoplastic; FEP
Material Notes: Dyneon FEP 6322 was designed primarily for high-speed extrusion for wire insulation. Its distinguishing features include:- High extrusion speed
- High thermal stability
- Wide processing window
- Superior electrical properties
- Excellent low smoke and low flame properties
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Melt Index of Compound
- Tensile Strength at Break
- Elongation at Break
- Izod Impact, Notched
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Melting Point
- Brittleness Temperature
- Flammability, UL94
- Oxygen Index
|
|
|
|