Dyneon™ Fluorothermoplastics FEP X 6301 UHP Fluorinated Ethylene Propylene
Subcategory: Fluoropolymer; Thermoplastic; FEP
Material Notes: Dyneon FEP X 6301 UHP was designed primarily for ultra-high purity applications requiring very low levels of metals and ions. This extrusion grade of EEP is ideally suited for tubing, which can be used in applications such as chemical transport, heat exchangers, ect. Distinguishing features of this grade include:- extremely low levels of extractable ions
- Wide service temperature range
- excellent thermal stability
- smooth surfaces
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Melt Index of Compound
- Tensile Strength at Break
- Elongation at Break
- Melting Point
|
|
|
|