Dyneon™ Fluorothermoplastics PFA 6502TA Perfluoroalkoxy
Subcategory: Fluoropolymer; Thermoplastic; PFA
Material Notes: Dyneon PFA 6502TA is a new fluorothermoplastic resin developed for compression molding applications. PFA 6502TA has a wide processing window with excellent color stability when longer residence times or higher temperatures are required.Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Bulk Density
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Oxygen Index
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|