Dyneon™ Fluorothermoplastics THV 340C
Subcategory: Fluoropolymer; Thermoplastic
Material Notes: THV 340C is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of concentrated water-based dispersion containing an ionic emulsifier. It provides a balance of low temperature processing, low flammability, thermal stability, and melt processability. It is designed for coating heat sensitive substrates such as polyester fabrics with its lower fusion temperature and high melt flow index to improve penetration and reflow. It provides a good balance of flexibility, weatherability, chemical resistance, and soil resistance properties in a water-based formulation. No plasticizers are added to achieve flexibility.Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Solids Content
- Melt Index of Compound
- Melting Point
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|