Dyneon™ Fluorothermoplastics THV 815G
Subcategory: Fluoropolymer; Thermoplastic
Material Notes: Dyneon THV 815 G provides a balance of low permeation, thermal stability, and melt processability. IT can be used to prepare molded parts and extruded films, tubes, profiles, and wire coatings. It is useful for applications that require flexibility and good chemical resistance. This product processes at higher temperature than that of previous THV grades; therefore, the use of corrosion-resistant equipment is suggested.Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Melt Index of Compound
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Form
|
|
|
|
| Property Data |