Dyneon™ Fluorothermoplastics THVP 2030G X
Subcategory: Fluoropolymer; Thermoplastic
Material Notes: THVP 2030G X is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluoropolymer but need excellent flexibility or excellent transparency. THVP 2030G X is processed at low temperatures, but exhibits a slightly higher melt point and end-use temperature capability than THV 220.Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Bulk Density
- Melt Index of Compound
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Compression Set
- Melting Point
- Refractive Index
- Transmission, Visible
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|