Dyneon™ TF 1645 PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes:
- Meets ASTM D4894 Type IV, Grade 2 resin
- Molding and ram extrusion powder very good free-flow properties
- Good metering properties
- Good mold filling behavior
- Good electrical and mechanical properties
- Used in automatic, isostatic and general compression molding
- Excellent for finished molded parts
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Bulk Density
- Particle Size
- Deformation
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Dielectric Strength
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Shrinkage
|
|
|
|
| Property Data |