Dyneon™ TFM™ 1700 PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes:
- Meets ASTM D4894 Type III, Grade 1 resin
- Non-free-flowing compression molding powder
- Very fine particle size
- Dense polymer structure, low permeability
- Improved weldability
- Low deformation under load
- Good electrical and mechanical properties
- Increased modulus of elasticity
- Low molding pressure
- Excellent for production of very thin films with superior permeation properties
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Bulk Density
- Particle Size
- Deformation
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Dielectric Strength
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|