Dyneon™ TF 2021 PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes:
- Processable by standard paste extrusion methods
- Both grades can be processed at low to medium reduction ratios
- TF 2021 PTFE is preferred for unsintered thread sealing tapes and expanded joint sealants
- TF 2025 PTFE is recommended for pipe liner and applications because of its superior green strength
Information provided by Dyneon, A 3M Company
| Available Properties |
- Density
- Bulk Density
- Particle Size
- Tensile Strength at Break
- Elongation at Break
- Extrusion Pressure, Mpa
- Reduction Ratio Range (Dyneon Method)
|
|
|
|