Dyneon™ TF 9201 PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes:
- Low molecular weight virgin PTFE (non-degraded)
- Agglomerate particles
- Easily deagglomerated when incorporated into other matrixes
- Suitable for use in food contact applications. Complies with FDE specification 21 CFR 177.1550
Information provided by Dyneon, A 3M Company
| Available Properties |
- Bulk Density
- Particle Size
- Specific Surface Area
- Viscosity
- Melt Flow
- Primary Particle Size g/l
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|