Dyneon™ TF 5050R PTFE
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Material Notes:
- Bimodal particle size distribution
- Low settling temperature
- Excellent film-forming properties
- Low porosity
- High gloss
- Greater hardness
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Solids Content
- Particle Size
- pH
- Viscosity
- Emulsifier
- Emulsifier Content %
|
|
|
|