Dyneon™ Fluoroplastic PVDF 11008/0003 Polyvinylidene Fluoride
Subcategory: Fluoropolymer; Thermoplastic; PVDF
Material Notes:
- Dyneon PVDF 11008/0003 is a copolymer of VF2 and HFP
- Improved flexibility over PVDF homopolymers
- Very low smoke and low flame generation
- Ideal for applications where high strength and a moderate degree of flexibility are required
- Ideal for high speed extrusion
- Excellent weatherability
- Good chemical resistance
- Long term use temperatures up to 150°C
- Processable using most conventional thermoplastic conversion techniques
Information provided by Dyneon, A 3M Company
| Available Properties |
- Density
- Water Absorption
- Melt Index of Compound
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Melting Point
- Flammability, UL94
- Oxygen Index
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|