Dyneon™ Fluoroplastic PVDF 31508/0003 Polyvinylidene Fluoride
Subcategory: Fluoropolymer; Thermoplastic; PVDF
Material Notes:
- Copolymer of VF2 and CTFE
- Ultra-flexible
- Very low shrinkage rates
- Wide operating temperature window
- Processable using a variety of thermoplastic conversion techniques
- Excellent low flame and low smoke performance
Information provided by Dyneon, A 3M Company