Dyneon™ Fluoroelastomer FC 2182
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes:
- Composition: di-polymer of vinylidene fluoride and hexafluoropropylene
- Low viscosity
- Process targets: injection and transfer molding, and extrusion
- Proprietary incorporated cure technology
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- Compression Set
- Transformation Temperature
- 5`50, Time to 50% cure, minutes
- Color
- MH, Maximum Torque, inch-lb @ 177°C
- ML, Minimum Torque inch-lb @ 177°C
- Solubility
- t`90 - Time to 90% cure @ 177°C - minutes
- ts2 - Time to 2 in-lb rise from min @ 177°C - min
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|