Dyneon™ Fluoroelastomer FC 2210X 80/20
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Dyneon FC 2210X is an ultra low viscosity fluoroelastomer. It is a 65% fluorine di-polymer with no incorporated cure and a viscosity of 200 poise at 105°C. Dyneon is packaged in two easy-to-use forms: 35 pound cardboard boxes with release liners for easy removal and five gallon metal pails also containing 25 pounds of product. The boxes are ideal for milling processes and the pails can easily be heated in an oven so product can be dispensed by pouring.Information provided by Dyneon, A 3M Company
| Available Properties |
- Mooney Viscosity
- Carbon Black Loading
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Fracture Toughness
- Compression Set
- Ca(OH)2 wt. %
- Dyneon™ FC 2174 wt.%
- Dyneon™ FC 2210X wt.%
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|