Dyneon™ Fluoroelastomer FC 2211
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes: Dyneon FC 2211 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formulations. The "dry" ingredients should be blended before adding to masticated gum. For best results, FC 2211 should be branded on the mill several minutes prior to adding the blended dry ingredients. Once mixed, the compounded stocks have good scorch resistance and storage stability.Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- Compression Set
- Transformation Temperature
- 5`50, Time to 50% cure, minutes
- Color
- MH, Maximum Torque, inch-lb @ 177°C
- ML, Minimum Torque inch-lb @ 177°C
- Solubility
- t`90 - Time to 90% cure @ 177°C - minutes
- ts2 - Time to 2 in-lb rise from min @ 177°C - min
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|