Dyneon™ Fluoroelastomer FLS 2650
Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset
Material Notes:
- Composition: Terpolymer of vinylidene fluoride, hexafluoropropylene, and tetrafluoroethylene; plus cure site monomer
- Low volume swell high fluorine terpolymer
- Can be used in blends with fluorosilicone, silicone, EDPM and other peroxide curable elastomers
- Process targets: transfer and compression molding
- Slightly improved water and steam resistance over conventional fluoroelastomer
- Vulcanization of thick cross-section parts without fissuring
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- Compression Set
- Transformation Temperature
- 5`50, Time to 50% cure, minutes
- Color
- MH, Maximum Torque, inch-lb @ 177°C
- ML, Minimum Torque inch-lb @ 177°C
- Solubility
- t`90 - Time to 90% cure @ 177°C - minutes
- ts2 - Time to 2 in-lb rise from min @ 177°C - min
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|