Dyneon™ Elastomer Additive FC 2172P
Subcategory: Fluoropolymer, TS; Additive/Filler for Polymer
Material Notes: Dynamar FC 2172P is a cure accelerator masterbatch for use with all incorporated cure fluoropolymers. FC 2172P in fluoroelastomer formulations provides- Fast cure rates at reduced molding temperatures of 150-165°C
- Slightly accelerated cure rates at normal molding temperatures of 180-190°C
- A way to adjust cure speeds of fluoroelastomer compounds that contain fillers which tend to have a "retarding" effect
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- Compression Set
- Color
- Solubility
|
|
|
|
| Property Data |