Dyneon™ Polymer Processing Additives FX 5911
Subcategory: Fluoropolymer, TS; Additive/Filler for Polymer
Material Notes: Dynamar FX 5911 is a free-flowing fluoropolymer processing aid that is designed for use at very low levels (typically 250-1000 ppm) necessary to improve processing, it does not alter or detract from the good physical properties associated with high strength plastics. Features and Benefits - Broadens extrusion processing capabilities of polyolefin resins
- Reduces or eliminates die build-up
- Ideal for use in high viscosity, high molecular weight polyolefins
- Excellent thermal stability for high temperature processing
- Lowers apparent melt viscosity
- For use at very low levels
- Free-flowing fluoropolymer processing aid
- Can offer performance and cost advantages
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Particle Size
- Melt Index of Compound
- Melting Point
- Active Ingredients (%)
- Color
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|