Dyneon™ Polymer Processing Additives FX 5912
Subcategory: Fluoropolymer, TS; Additive/Filler for Polymer
Material Notes: Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm have demonstrated benefits in specialized extrusion, and calendering processes. Features and Benefits - Process targets: Extrusion and processing of wire and cable, fiber spinning, and certain calendering operations
- Broadens extrusion processing capabilities of certain types of polyolefin resins
- Excellent thermal stability
- Effective as a process aid over a broad process temperature range
- Free flowing granular product form
- 100% active
- Reduces/eliminates die build-up
- Lowers apparent melt viscosity
- For use at very low levels
- Can offer performance and cost advantages
Information provided by Dyneon, A 3M Company
| Available Properties |
- Specific Gravity
- Particle Size
- Melt Index of Compound
- Melting Point
- Active Ingredients (%)
- Color
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|