Dyneon™ Polymer Processing Additives FX 9613
Subcategory: Fluoropolymer, TS; Additive/Filler for Polymer
Material Notes: Dynamar polymer processing additive FX 9613 is a free flowing granular concentrate form of a fluoropolymer designed for use at very low levels to improve the processing of thermoplastics. At the very low use levels (typically 50 - 1000 ppm) necessary to improve processing, it does not alter or detract from the good mechanical properties associated with high strength plastics.Features and Benefits - Broadens extrusion processing capabilities of polyolefin resins
- Ideal for use in low melt index LLDPE and high molecular weight HDPE resins
- Excellent thermal stability for high temperature processing
- Reduces or eliminates melt fracture
- Reduces or eliminates die build-up
- Lowers apparent melt viscosity
- For use at very low levels
- Free-flowing fluoropolymer based processing aid
- Can offer performance and cost advantages
Information provided by Dyneon, A 3M Company
| Available Properties |
- Bulk Density
- Particle Mesh Size
- Color
- Form
- Inorganic Additives %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|