Dymax 425 Light Weld® High Clarity Glass Bonding Adhesive
Subcategory: Adhesive; Thermoset
Material Notes:
Glass Bonding in Seconds Description
Dymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bonding applications, Light Weld 400 Series are excellent, cost effective replacements for optical cements. Adhesives are dishwasher safe, non-yellowing (UV resistant) and exhibit low shrinkage.
Features and Benefits
- 1 to 60 second cures
- Solvent-free; no ozone depleting chemicals (O.D.C.s), low V.O.C.s
- Thermal shock -55°C to 150°C
- Structural adhesion to 4,000 psi
- 100% in-line Q.C.
- Better worker acceptance and low regulatory cost
- Dishwasher safe
- Ideal for demanding applications
Dymax 425 Light Weld® High Clarity Glass Bonding Adhesive Typical Use: Stemware, L.E.D., coatings, dishwasher resistant
| Available Properties |
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Refractive Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|