Dymax 3-20522 Fast Shallow Potting Compound and Sealant

 

Subcategory: Adhesive; Thermoset

Material Notes:

Shallow Potting and Sealing in Seconds
Features

  • UV cures in seconds to 1/4 inch deep
  • One component, no mixing
  • Solvent-free
  • Environmentally friendly
  • Excellent adhesion to most substrates

Description

UV curable potting materials are used for sealing electrical connectors, temperature probes and sensors in applications throughout the aerospace, electronic, electrical, industrial, defense and marine industries. Dymax pitting compounds cure in seconds, on demand, and have very low shrinkage. See pages for a selection of Dymax UV curing lamps and conveyors which can dramatically lower production costs when used in conjunction with Dymax adhesives.

Dymax 3-20522 Fast Shallow Potting Compound and Sealant
Translucent bonds with high adhesion; cures to 1/8 inch Key Substrates: ABS, Filled Nylon, Metal, Glass Typical Use: For inductor and larger area potting

Available Properties

We're sorry, but our sources do not report
any other information for this material.

  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。